Ferro Frit 3211

Calcium Borate Frit

Alternate Names: F3211

OxideAnalysisFormula
CaO42.00%1.000
B2O358.00%1.113
Oxide Weight133.57
Formula Weight133.57
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.5
MLRG - Frit Melting Range (C) 1750F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3211" descrip="Calcium Borate Frit" searchkey="F3211" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="42.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="58.000" tolerance=""/> </oxides> </material>