Ferro Frit 3193

Alkaline borate bonding frit for abrasive industry

OxideAnalysisFormula
CaO10.70%0.518
K2O2.60%0.075
Na2O9.30%0.407
Al2O37.81%0.208
B2O315.60%0.609
SiO254.00%2.439
Oxide Weight271.52
Formula Weight271.52
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3193" descrip="Alkaline borate bonding frit for abrasive industry" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.810" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved