Ferro Frit 3191

A source of alkali borate for use in abrasives industry

Alternate Names: F3191

OxideAnalysisFormula
CaO11.27%0.500
Na2O12.46%0.500
B2O327.97%1.000
SiO248.30%2.000
Oxide Weight248.84
Formula Weight248.84
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.2 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1300F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3191" descrip="A source of alkali borate for use in abrasives industry" searchkey="F3191" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.270" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.460" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="27.970" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved