Ferro Frit 3185

Low melting alkali borate bonding frit for abrasives

Alternate Names: F3185

OxideAnalysisFormula
Na2O7.70%1.000
B2O338.20%4.419
SiO254.10%7.248
Oxide Weight805.19
Formula Weight805.19
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.10
MLRG - Frit Melting Range (C) 1350F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3185" descrip="Low melting alkali borate bonding frit for abrasives" searchkey="F3185" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="38.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.100" tolerance=""/> </oxides> </material>