Ferro Frit 271D

Clear cone 6 dinnerware glaze frit

Alternate Names: Frit KMG 271D

OxideAnalysisFormula
CaO9.19%0.620
MgO0.12%0.011
K2O0.17%0.007
Na2O5.22%0.319
ZnO0.47%0.022
SrO0.08%0.003
P2O50.01%0.000
PbO1.09%0.018
TiO20.12%0.006
Al2O311.99%0.445
B2O313.00%0.707
SiO255.52%3.495
Fe2O30.12%0.003
LOI1.74
Oxide Weight367.40
Formula Weight373.90
If this formula is not unified correctly please contact us.

A midfire - range low COE 1050 - 1150 C clear glaze, mainly used for commercial dinnerware. It was only made for sale in Australia and New Zealand.

This analysis 97 and seems to have too many oxides so it may not be accurate.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 271D" descrip="Clear cone 6 dinnerware glaze frit" searchkey="Frit KMG 271D" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.190" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.120" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.170" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.220" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.470" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="0.080" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.010" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="1.090" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.120" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.990" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.520" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.120" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.740" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved