Ferro Frit 1212

Alkali borosilicate frit

OxideAnalysisFormula
Na2O15.60%1.000
Al2O35.10%0.199
B2O326.30%1.502
SiO252.90%3.498
Oxide Weight397.04
Formula Weight397.04
If this formula is not unified correctly please contact us.

This is not a replacement for Colemanite as claimed by some.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 1212" descrip="Alkali borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved