Ferro Feldspar No. 10

Legacy feldspar

Alternate Names: Ferro Feldspar #10

OxideAnalysisFormula
K2O9.84%0.714
Na2O2.59%0.286
Al2O314.64%0.982
SiO268.83%7.832
LOI4.10
Oxide Weight655.80
Formula Weight683.84
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Feldspar No. 10" descrip="Legacy feldspar" searchkey="Ferro Feldspar #10" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="9.840" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.590" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="14.640" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.830" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="4.100" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved