Feldspar Holguín (Cuba)

Cuban feldspar

OxideAnalysisFormula
CaO2.20%0.267
MgO0.48%0.081
K2O1.22%0.088
Na2O5.15%0.565
TiO20.01%0.001
Al2O317.18%1.145
SiO271.90%8.131
Fe2O30.31%0.013
LOI1.00
Oxide Weight669.08
Formula Weight675.84
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Feldspar Holguín (Cuba)" descrip="Cuban feldspar" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.480" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.220" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.150" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.180" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="71.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.310" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved