Feldspar 635

Alternate Names: Feldspat 635

OxideAnalysisFormula
CaO0.79%0.085
MgO0.34%0.051
K2O0.32%0.021
Na2O8.62%0.843
TiO20.13%0.010
Al2O316.30%0.969
SiO272.84%7.348
Fe2O30.11%0.004
LOI0.55
Oxide Weight602.92
Formula Weight606.25
If this formula is not unified correctly please contact us.

Available in 10, 25 and 50mm sizes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Feldspar 635" descrip="" searchkey="Feldspat 635" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.790" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.340" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.320" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.620" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.130" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="72.840" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.110" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.550" tolerance=""/> </volatiles> </material>