Feldspar 632

Alternate Names: Feldspat 632

OxideAnalysisFormula
CaO0.60%0.057
MgO0.16%0.021
K2O1.21%0.069
Na2O9.85%0.852
TiO20.28%0.019
Al2O320.15%1.060
SiO267.28%6.006
Fe2O30.17%0.006
LOI0.30
Oxide Weight534.92
Formula Weight536.53
If this formula is not unified correctly please contact us.

Available in 10, 25 and 50mm sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Feldspar 632" descrip="" searchkey="Feldspat 632" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.600" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.160" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.210" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.850" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.280" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="20.150" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="67.280" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.170" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved