F7/SG Feldspar

Soda Feldspar

OxideAnalysisFormula
CaO0.49%0.050
MgO0.05%0.007
K2O0.47%0.029
Na2O9.90%0.914
TiO20.02%0.001
Al2O317.40%0.977
SiO270.80%6.745
Fe2O30.24%0.009
LOI0.60
Oxide Weight568.99
Formula Weight572.43
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.65
HMOH - Hardness (Moh) 6.5
BDGC - Bulk Density g/cc (Packed) 1.2
UPSD - Ultimate Particle Size Distribution >71 micron: 1.2%
pHPW - pH for dry powder 8-9

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="F7/SG Feldspar" descrip="Soda Feldspar" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.490" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.470" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.900" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.020" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.240" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved