F7/SE Feldspar

Soda Feldspar

Alternate Names: Feldspar Soda F7/SE

OxideAnalysisFormula
CaO0.55%0.055
MgO0.05%0.007
K2O0.28%0.017
Na2O10.20%0.921
TiO20.06%0.004
Al2O317.50%0.961
SiO270.80%6.598
Fe2O30.12%0.004
LOI0.36
Oxide Weight557.66
Formula Weight559.67
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.65
HMOH - Hardness (Moh) 6.5
BDGC - Bulk Density g/cc (Packed) 1.2
UPSD - Ultimate Particle Size Distribution >71 micron: 1%
pHPW - pH for dry powder 8-9

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="F7/SE Feldspar" descrip="Soda Feldspar" searchkey="Feldspar Soda F7/SE" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.550" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.280" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.060" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.120" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.360" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved