F-20 Feldspar

Potash/sodium/calcium 20 mesh Feldspar

Alternate Names: F20 Feldspar

OxideAnalysisFormula
CaO1.40%0.140
K2O4.10%0.244
Na2O6.82%0.616
Al2O318.85%1.035
SiO268.15%6.353
Fe2O30.07%0.002
LOI0.08
Oxide Weight556.87
Formula Weight557.32
If this formula is not unified correctly please contact us.
SADR - Sieve Analysis Dry Cumulative: +30 mesh 1.8 +40 mesh 15.9 +200 mesh 94.7 -200 mesh 5.3
BDLB - Bulk Density lbs/cu. ft. (Packed) 80

F-20 Feldspar is a high quality sodium/ Potassium/calcium aluminum silicate used principally as a flux for ceramic applications. Carefully beneficiated using the froth flotation process, F-20 Feldspar offers high levels of alkali oxides per unit of alumina with low iron oxide content.

Suitable for all types of glazes
Max Firing Temp: over 1250C


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="F-20 Feldspar" descrip="Potash/sodium/calcium 20 mesh Feldspar" searchkey="F20 Feldspar" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.820" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.850" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.150" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.080" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved