Excelsior Ball Clay

Highly plastic ball clay

OxideAnalysisFormula
CaO0.30%0.016
MgO0.30%0.022
K2O1.20%0.037
Na2O0.20%0.009
TiO21.30%0.047
Al2O335.00%1.000
SiO249.00%2.376
Fe2O31.60%0.029
SO411.00
Oxide Weight259.08
Formula Weight291.10
If this formula is not unified correctly please contact us.

Highly plastic ball clay blend designed for high strength at moderate specific surface area levels.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Excelsior Ball Clay" descrip="Highly plastic ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="35.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="11.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved