Eureka Feldspar

Legacy low calcium potash feldspar

OxideAnalysisFormula
CaO0.01%0.001
K2O9.37%0.638
Na2O3.49%0.361
Al2O317.05%1.072
SiO269.70%7.437
Fe2O30.11%0.004
LOI0.20
Oxide Weight639.55
Formula Weight640.83
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Eureka Feldspar" descrip="Legacy low calcium potash feldspar" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.010" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="9.370" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.490" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.050" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.110" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved