Eucalyptus Ash

Washed

OxideAnalysisFormula
CaO20.26%0.374
MgO11.94%0.307
K2O10.33%0.114
Na2O10.83%0.181
P2O53.41%0.025
Al2O32.21%0.022
SiO232.90%0.567
Fe2O33.50%0.023
MnO0.51%0.007
SO34.11
Oxide Weight99.29
Formula Weight103.54
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Eucalyptus Ash" descrip="Washed" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="20.260" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="11.940" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.330" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.830" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="3.410" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.210" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.500" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.510" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO3" name="Sulfur Trioxide" percent="4.110" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved