Esmalglass Frit FT 8547

Alternate Names: Esmalglass Frit 8547

OxideAnalysisFormula
BaO0.10%0.001
CaO14.90%0.570
MgO1.20%0.064
K2O5.40%0.123
Na2O0.90%0.031
ZnO7.90%0.208
P2O50.10%0.002
Al2O37.50%0.158
SiO260.50%2.162
Fe2O30.10%0.001
LOI0.60
Oxide Weight211.76
Formula Weight213.04
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 1090C
MLRG - Frit Melting Range (C) 1170C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FT 8547" descrip="" searchkey="Esmalglass Frit 8547" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.900" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.900" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.900" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved