Esmalglass Frit FT 821/6

Alternate Names: Esmalglass Frit 821/6

OxideAnalysisFormula
BaO0.20%0.003
CaO12.80%0.523
MgO1.50%0.085
K2O5.30%0.129
Na2O0.90%0.033
ZnO7.70%0.217
SrO0.10%0.002
P2O50.10%0.002
PbO0.60%0.006
TiO20.10%0.003
Al2O38.40%0.189
SiO261.00%2.326
Fe2O30.10%0.001
ZrO20.30%0.006
LOI0.70
Oxide Weight227.07
Formula Weight228.67
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 1060C
MLRG - Frit Melting Range (C) 1145C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FT 821/6" descrip="" searchkey="Esmalglass Frit 821/6" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.200" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.800" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.900" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.700" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="0.100" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.100" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="0.600" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved