Esmalglass Frit FO 963

OxideAnalysisFormula
CaO10.20%0.390
MgO3.60%0.192
K2O5.20%0.118
Na2O0.50%0.017
ZnO10.70%0.282
Al2O35.60%0.118
SiO256.60%2.022
Fe2O30.10%0.001
ZrO27.60%0.132
Oxide Weight214.87
Formula Weight214.87
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 940C
MLRG - Frit Melting Range (C) 1170C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FO 963" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved