Esmalglass Frit FO 940/1

OxideAnalysisFormula
BaO0.20%0.002
CaO20.10%0.594
MgO8.40%0.346
K2O1.10%0.019
Na2O1.00%0.027
ZnO0.50%0.010
SrO0.10%0.002
Al2O319.80%0.322
SiO246.00%1.269
Fe2O30.10%0.001
ZrO20.40%0.005
LOI0.60
Oxide Weight162.04
Formula Weight163.02
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 910C
MLRG - Frit Melting Range (C) 1245C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FO 940/1" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.200" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="20.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="8.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.500" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.400" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved