Esmalglass Frit FO-961/P

OxideAnalysisFormula
CaO9.20%0.334
MgO3.80%0.192
K2O5.50%0.119
Na2O0.30%0.010
ZnO13.30%0.333
P2O50.80%0.011
TiO20.10%0.003
Al2O35.20%0.104
SiO253.40%1.811
Fe2O30.10%0.001
ZrO27.40%0.122
LOI0.60
Oxide Weight202.02
Formula Weight203.24
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 960C
MLRG - Frit Melting Range (C) 1170C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FO-961/P" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="13.300" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.800" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.400" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.400" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved