Esmalglass Frit FM 86

OxideAnalysisFormula
BaO0.80%0.011
CaO12.80%0.490
MgO0.50%0.027
K2O4.00%0.091
Na2O1.50%0.052
ZnO11.90%0.314
SrO0.30%0.006
P2O50.10%0.002
PbO0.70%0.007
Al2O319.60%0.413
SiO245.90%1.641
Fe2O30.10%0.001
ZrO20.60%0.010
LOI0.50
Oxide Weight212.30
Formula Weight213.37
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 855C
MLRG - Frit Melting Range (C) 1180C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FM 86" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.800" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.800" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="11.900" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="0.300" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.100" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="0.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved