Esmalglass Frit FM 1403/G

OxideAnalysisFormula
BaO0.50%0.010
CaO5.60%0.310
MgO1.60%0.123
K2O5.40%0.178
Na2O1.20%0.060
ZnO2.70%0.103
SrO7.00%0.210
PbO0.30%0.004
Al2O321.00%0.640
SiO253.00%2.743
Fe2O30.10%0.002
ZrO20.10%0.003
LOI0.60
Oxide Weight306.33
Formula Weight308.18
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 950C
MLRG - Frit Melting Range (C) 1285C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esmalglass Frit FM 1403/G" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.600" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.700" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved