Esan Feldspar

Turkish Soda Feldspar

Alternate Names: ESF501FG

OxideAnalysisFormula
CaO0.30%0.031
MgO0.20%0.028
K2O0.30%0.018
Na2O10.00%0.923
TiO20.05%0.004
Al2O318.00%1.010
SiO270.00%6.664
Fe2O30.05%0.002
LOI0.30
Oxide Weight565.84
Formula Weight567.54
If this formula is not unified correctly please contact us.
UPSD - Ultimate Particle Size Distribution +200 3.50 +100 13.00 +74 24.50 +63 6.00 +45 13.00 -45 40.00

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Esan Feldspar" descrip="Turkish Soda Feldspar" searchkey="ESF501FG" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.000" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.050" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.050" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved