Dolocron 40-13

325 mesh Dolomite, CaMg(CO3)2

OxideAnalysisFormula
CaO30.42%0.500
MgO21.85%0.500
Fe2O30.30%0.002
LOI47.40
Oxide Weight48.48
Formula Weight92.16
If this formula is not unified correctly please contact us.

Produced in Canaan, CT. A pulverized dolomitic limestone (calcium-magnesium carbonate). Used in many industries.

The 40-13 designation means the largest particle size is 40 microns (325 mesh) and the oil absorption is 13 grams/100 grams.
This material is 55% CaCO3 and 43% MgCO3, 0.3% Fe2O3.
Specific gravity: 2.8
Bulk density: 1.04 g/cc (65 lbs/cubic ft)


Dolocron Dolomite

Dolocron Dolomite

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Dolocron 40-13" descrip="325 mesh Dolomite, CaMg(CO3)2" searchkey="" loi="0.00" casnumber="69598-19-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="30.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="21.850" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="47.400" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved