Degussa Frit 90368

Alternate Names: Frit D-90368, Erdalkaliborsilikat D 90368

OxideAnalysisFormula
CaO18.24%0.700
MgO1.87%0.100
Na2O5.76%0.200
Al2O311.84%0.250
B2O36.46%0.200
SiO255.82%2.000
Oxide Weight215.29
Formula Weight215.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 76 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 630C 830C 1080C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90368" descrip="" searchkey="Frit D-90368, Erdalkaliborsilikat D 90368" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="18.240" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.870" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.760" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.840" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.460" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.820" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved