Degussa Frit 90352

OxideAnalysisFormula
CaO7.09%0.200
Na2O3.92%0.100
ZnO28.27%0.550
PbO21.14%0.150
Al2O33.22%0.050
B2O32.20%0.050
SiO234.16%0.900
Oxide Weight158.32
Formula Weight158.32
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 60 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 483C 730C 970C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90352" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.090" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.920" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="28.270" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="21.140" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.220" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.160" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved