Degussa Frit 90328

OxideAnalysisFormula
CaO0.24%0.050
MgO0.35%0.101
Na2O4.52%0.849
Al2O37.88%0.900
B2O321.50%3.598
SiO265.51%12.694
Oxide Weight1164.60
Formula Weight1164.60
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 48 X 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 495C 795C 1270C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90328" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.240" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.350" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.520" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.880" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.510" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved