Degussa Frit 90321

Zinkbarium-fritte

Alternate Names: Zinkbarium fritte

OxideAnalysisFormula
BaO27.77%0.400
ZnO14.74%0.400
PbO20.21%0.200
Al2O34.62%0.100
SiO232.66%1.200
Oxide Weight220.86
Formula Weight220.86
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 99 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 507C 770C 980C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90321" descrip="Zinkbarium-fritte" searchkey="Zinkbarium fritte" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="27.770" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="14.740" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="20.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.620" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.660" tolerance=""/> </oxides> </material>