Degussa Frit 90187

Bienatriumbor-silikat

OxideAnalysisFormula
Na2O10.25%0.500
PbO36.91%0.500
B2O323.02%1.000
SiO229.82%1.500
Oxide Weight302.40
Formula Weight302.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 94 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 499C 590C 680C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90187" descrip="Bienatriumbor-silikat" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.250" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="36.910" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.020" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="29.820" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved