Degussa Frit 90176

Oxide Analysis Formula
SiO2 56.35% 4.00
B2O3 16.31% 1.00
CaO 9.86% 0.75
K2O 5.52% 0.25
Al2O3 11.95% 0.50
Oxide Weight 426.66
Formula Weight 426.66

Related Information

Links

Typecodes Frit

Data

Co-efficient of Linear Expansion56 x 10-7 (20-400C)
Heating Microscope Analysis for Frits600C
Heating Microscope Analysis for Frits865C
Heating Microscope Analysis for Frits1050C