Degussa Frit 90167

High alkali borosilicate frit

Alternate Names: Alkaliborfritte

OxideAnalysisFormula
CaO2.28%0.100
K2O17.21%0.450
Na2O11.33%0.450
Al2O38.28%0.200
B2O316.96%0.600
SiO243.93%1.800
Oxide Weight246.23
Formula Weight246.23
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 150 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 455C 646C 740C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90167" descrip="High alkali borosilicate frit" searchkey="Alkaliborfritte" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.280" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="17.210" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.330" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.280" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.960" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.930" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved