Degussa Frit 90158

Natriubor-Silikat

Alternate Names: 90158 Natriumborsilikat

OxideAnalysisFormula
Na2O16.25%1.000
B2O336.49%2.000
SiO247.26%3.000
Oxide Weight381.54
Formula Weight381.54
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 85 X 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 514C 685C 780C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90158" descrip="Natriubor-Silikat" searchkey="90158 Natriumborsilikat" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="16.250" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="36.490" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.260" tolerance=""/> </oxides> </material>