Degussa Frit 90155

Alkalizinkoor-fritte

Alternate Names: 90155 Alkalizinkborfritte

OxideAnalysisFormula
CaO10.73%0.400
Na2O5.93%0.200
ZnO15.56%0.400
Al2O37.31%0.150
B2O311.64%0.350
SiO248.83%1.700
Oxide Weight209.18
Formula Weight209.18
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 69 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 548C 770C 890C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90155" descrip="Alkalizinkoor-fritte" searchkey="90155 Alkalizinkborfritte" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.730" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.930" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="15.560" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.310" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.640" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.830" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved