Alternate Names: 90142 Calziumboratfritte

OxideAnalysisFormula
CaO25.71%1.000
Al2O39.35%0.200
B2O331.89%1.000
SiO233.05%1.200
Oxide Weight218.20
Formula Weight218.20
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 66 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 632C 900C 960C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90142" descrip="Calziumborat-fritte" searchkey="90142 Calziumboratfritte" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="25.710" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.350" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="31.890" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="33.050" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved