Degussa Frit 90062

Bleiborsilikat

Alternate Names: 90062 Bleiborsilikat

OxideAnalysisFormula
PbO62.41%1.000
B2O329.19%1.500
SiO28.40%0.500
Oxide Weight357.63
Formula Weight357.63
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion
Sp VAL
1 79 x 10-7 (20-400C)
HMA - Heating Microscope Analysis for Frits
Sp SP EP K HK F
1 440C 550C 640C    

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 90062" descrip="Bleiborsilikat" searchkey="90062 Bleiborsilikat" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="62.410" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.190" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="8.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved