•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Degussa Frit 15098

Frit used in crystalline glazes

OxideAnalysisFormula
CaO5.05%0.280
Li2O0.86%0.090
K2O10.60%0.350
ZnO7.33%0.280
Al2O311.48%0.350
B2O33.58%0.160
SiO261.09%3.162
Oxide Weight311.06
Formula Weight311.06
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Degussa Frit 15098" descrip="Frit used in crystalline glazes" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.050" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.860" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.330" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.480" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.580" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.090" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved