Crenshaw Ball Clay

Oxide Analysis Formula
CaO 0.30% 0.02
K2O 0.60% 0.02
MgO 0.40% 0.04
Na2O 0.10% 0.01
TiO2 1.50% 0.07
Al2O3 26.10% 1.00
SiO2 59.50% 3.87
Fe2O3 1.50% 0.04
LOI10.00%
Oxide Weight 351.72
Formula Weight 390.80

Related Information

Links

Materials Ball Clay
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.