Crecer Frit 804

Sodium medium borate frit

OxideAnalysisFormula
CaO6.50%0.305
MgO0.60%0.039
K2O3.60%0.101
Na2O13.05%0.555
TiO20.10%0.003
Al2O39.30%0.240
B2O311.00%0.417
SiO254.10%2.372
Fe2O30.28%0.005
LOI1.47
Oxide Weight259.66
Formula Weight263.54
If this formula is not unified correctly please contact us.

Fusion F43 has a little less KNaO but double the B2O3 and less SiO2. Ferro Frit 3110 is the opposite difference. You could calculate a combination of Frit 3110, Fusion F-43 and Kaolin that would be pretty close to this.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Crecer Frit 804" descrip="Sodium medium borate frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.050" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.280" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.470" tolerance=""/> </volatiles> </material>