Colorobia Frit F5

OxideAnalysisFormula
CaO11.00%0.395
K2O10.00%0.214
Na2O12.00%0.390
Al2O32.00%0.040
B2O338.00%1.101
SiO227.00%0.906
Oxide Weight201.70
Formula Weight201.70
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Colorobia Frit F5" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="38.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="27.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved