Colorobia Frit F4

OxideAnalysisFormula
CaO6.00%0.282
K2O9.00%0.251
Na2O11.00%0.467
Al2O39.00%0.232
B2O315.00%0.567
SiO250.00%2.190
Oxide Weight263.22
Formula Weight263.22
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Colorobia Frit F4" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="9.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.000" tolerance=""/> </oxides> </material>