Colorobbia Frit 335

Medium zinc opacified frit

OxideAnalysisFormula
CaO10.23%0.461
MgO3.28%0.206
K2O4.08%0.109
Na2O0.49%0.020
ZnO6.56%0.204
TiO20.08%0.003
Al2O37.11%0.176
SiO258.56%2.463
Fe2O30.14%0.002
ZrO27.89%0.162
LOI1.49
Oxide Weight248.82
Formula Weight252.58
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Colorobbia Frit 335" descrip="Medium zinc opacified frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.230" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.280" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.080" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.490" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="6.560" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.080" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.110" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.560" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.140" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.890" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.490" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved