Clay 246

OxideAnalysisFormula
CaO0.55%0.037
MgO0.70%0.065
K2O2.69%0.107
Na2O0.63%0.038
TiO21.21%0.057
Al2O327.11%1.000
SiO257.34%3.590
Fe2O31.16%0.027
SO40.12
LOI8.19
Oxide Weight343.85
Formula Weight375.01
If this formula is not unified correctly please contact us.
SADR - Sieve Analysis Dry > 41 micron: 0% > 30 micron: 0.45% > 20 micron: 2.79% > 10 micron: 20.3% < 3 micron: 37.55%
DS - Dry Strength (kgf/cm2) 25.23
FSHR - Firing Shrinkage 1150C: 6.13% 1200C: 7.34% 1250C: 7.34% 1325C: 8.14%

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Clay 246" descrip="" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.550" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.690" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.630" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="27.110" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.340" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.160" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.120" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="8.190" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved