Chrysanthos Frit FR005

High boron sodium frit

OxideAnalysisFormula
Na2O10.60%1.000
B2O323.95%2.013
SiO265.45%6.370
Oxide Weight584.91
Formula Weight584.91
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 980-1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Chrysanthos Frit FR005" descrip="High boron sodium frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.950" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.450" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved