Chrysanthos Frit FR004

Alumina lead bisilicate frit

OxideAnalysisFormula
PbO63.89%1.000
Al2O33.25%0.111
SiO232.96%1.916
Oxide Weight349.70
Formula Weight349.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 79
MLRG - Frit Melting Range (C) 850-900C
GTTM - Glass Transition Temperature 552C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Chrysanthos Frit FR004" descrip="Alumina lead bisilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="63.890" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.250" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.960" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved