Chrysanthos Frit FR003

High expansion alkali frit

OxideAnalysisFormula
BaO2.07%0.031
CaO5.77%0.238
MgO0.13%0.007
K2O5.60%0.137
Na2O15.72%0.586
Al2O35.90%0.134
B2O315.68%0.521
SiO249.13%1.890
Oxide Weight231.17
Formula Weight231.17
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 112
MLRG - Frit Melting Range (C) 900-950C
GTTM - Glass Transition Temperature 565C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Chrysanthos Frit FR003" descrip="High expansion alkali frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.070" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.770" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.130" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.720" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.680" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.130" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved