Ceram BBR clay

Alternate Names: Clay Ceram BBR

OxideAnalysisFormula
CaO0.13%0.008
MgO0.35%0.028
K2O0.51%0.018
Na2O0.19%0.010
P2O50.11%0.003
TiO21.20%0.049
Al2O331.20%1.000
SiO252.40%2.850
SO413.50
Oxide Weight281.45
Formula Weight325.37
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceram BBR clay" descrip="" searchkey="Clay Ceram BBR" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.130" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.350" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.510" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.190" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.110" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="31.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.400" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="13.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved