Ceraflux

Lead alumina bilsilicate frit (1% alumina)

Alternate Names: Lead alumina bisilicate

OxideAnalysisFormula
PbO65.00%1.000
Al2O31.00%0.034
SiO234.00%1.943
Oxide Weight343.38
Formula Weight343.38
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 4.6-4.65
MLRG - Frit Melting Range (C) 788-816C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceraflux" descrip="Lead alumina bilsilicate frit (1% alumina)" searchkey="Lead alumina bisilicate" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="65.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved