Ceradel Frit C 1255

Fritte zirconifere sans plomb, low expansion ziron frit

Alternate Names: Fritte C1255, Fritte C 1255, Ceradel Frit 1255

OxideAnalysisFormula
CaO5.85%0.375
K2O4.10%0.156
Na2O2.70%0.156
ZnO7.08%0.313
Al2O35.62%0.198
B2O312.11%0.625
SiO255.75%3.333
ZrO26.79%0.198
Oxide Weight359.29
Formula Weight359.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 58x10-7 (20/300C)
GSPT - Frit Softening Point 920-1020C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit C 1255" descrip="Fritte zirconifere sans plomb, low expansion ziron frit" searchkey="Fritte C1255, Fritte C 1255, Ceradel Frit 1255" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.850" tolerance="2"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance="2"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.700" tolerance="2"/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.080" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.620" tolerance="3"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.110" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.750" tolerance="15"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="6.790" tolerance="2.5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved