Ceradel Frit C 1254

Fritte calco-alcaline sans plomb

Alternate Names: Fritte C1254, Fritte C 1254, Ceradel Frit 1254

OxideAnalysisFormula
CaO10.15%0.500
Na2O11.22%0.500
Al2O37.38%0.200
B2O327.73%1.101
SiO243.51%2.000
Oxide Weight276.30
Formula Weight276.30
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 72x10-7 (20/300C)
GSPT - Frit Softening Point 800-920C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit C 1254" descrip="Fritte calco-alcaline sans plomb" searchkey="Fritte C1254, Fritte C 1254, Ceradel Frit 1254" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.150" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.220" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.380" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="27.730" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.510" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved